文章摘要
武军,马超,肖武,张朝忠,杨伟栋,沈海生,汪龙生,沈荣波.烟包防“水雾”研究[J].包装工程,2018,39(5):203-208.
WU Jun,MA Chao,XIAO Wu,ZHANG Chao-zhong,YANG Wei-dong,SHEN Hai-sheng,WANG Long-sheng,SHEN Rong-bo.Mist Resistance of Cigarette Packets[J].Packaging Engineering,2018,39(5):203-208.
烟包防“水雾”研究
Mist Resistance of Cigarette Packets
投稿时间:2017-01-25  修订日期:2018-03-10
DOI:10.19554/j.cnki.1001-3563.2018.05.038
中文关键词: 水雾  烟包  防水雾剂  防雾光油  物理化学协同效应
英文关键词: water mist  cigarette packet  anti-mist agent  anti-mist light oil  physical-chemical synergy
基金项目:
作者单位
武军 永发印务(东莞)有限公司东莞 523821 
马超 永发印务(东莞)有限公司东莞 523821 
肖武 永发印务(东莞)有限公司东莞 523821 
张朝忠 永发印务(东莞)有限公司东莞 523821 
杨伟栋 永发印务(东莞)有限公司东莞 523821 
沈海生 永发印务(东莞)有限公司东莞 523821 
汪龙生 永发印务(东莞)有限公司东莞 523821 
沈荣波 永发印务(东莞)有限公司东莞 523821 
摘要点击次数:
全文下载次数:
中文摘要:
      目的 为了解决烟包产品表面出现的“水雾”问题,分析纸张、光油、印刷品表面的印刷膜层、内装物烟丝等烟包产品的原材料和印刷工艺对“水雾”现象的影响。方法 通过减量法找到产生“水雾”的来源,创新一种上光油体系,采用以物理和化学协同的方法排除“水雾”。结果 当纳米二氧化硅的质量分数为0.15%、防水雾剂质量分数为0.15%共同作用时,彻底消除了“水雾”,同时发现当印刷品表面平滑度值为8000~14 000 s时满足对产品的质量要求。结论 包装盒的纸板、印刷UV油墨、光油等是“水雾”的主要来源,外层包覆的BOPP膜的密封性和外界温度变化提供了“水雾”形成的环境,而通过测定印刷品表面平滑度值可以判定水雾是否出现。
英文摘要:
      The work aims to solve the problem of "water mist" on the cigarette packet products, and analyze the effects of raw material of cigarette packet products (such as paper, varnish, printed film on the printed matter and cut tobacco) and printing technology on the "water mist". The sources of "water mist" were found by the weight loss method. The varnish system, with the use of physical-chemical synergy, was created to eliminate the "water mist". When the mass fraction of nano-silica was 0.15% and the mass fraction of anti-mist agent was 0.15%, the "water mist" was completely eliminated, and it was found that the product quality requirements were met when the surface smoothness of printed matter was 8000~14 000 s. The paperboards, printing UV ink and varnish, etc. of the packaging box are the sources of "water mist". The tightness of BOPP film coated on the outside and the change in external temperature provide the environment where the "water mist" is formed. It can be judged whether the water mist occurs by measuring the surface smoothness of printed matter.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第21231659位访问者    渝ICP备15012534号-2

版权所有:《包装工程》编辑部 2014 All Rights Reserved

邮编:400039 电话:023-68795652 Email: designartj@126.com

    

渝公网安备 50010702501716号