文章摘要
王子维,黎宇辉,童宇星,舒灏,刘奔,徐耀威,刘志昌,高颂,刘雄斌.稠浆法烟草薄片试制设备及热风定型质量控制[J].包装工程,2022,43(17):243-248.
WANG Zi-wei,LI Yu-hui,TONG Yu-xing,SHU HAO,LIU Ben,XU Yao-wei,LIU Zhi-chang,GAO Song,LIU Xiong-bin.Trial Production Equipment for Slurry Processed Reconstituted Tobacco and Quality Control of Heat Air Forming Process[J].Packaging Engineering,2022,43(17):243-248.
稠浆法烟草薄片试制设备及热风定型质量控制
Trial Production Equipment for Slurry Processed Reconstituted Tobacco and Quality Control of Heat Air Forming Process
  
DOI:10.19554/j.cnki.1001-3563.2022.17.032
中文关键词: 稠浆法  烟草薄片  试制设备  流热耦合
英文关键词: slurry processed reconstituted tobacco  tobacco sheet  trial production equipment  fluid-thermal coupling
基金项目:
作者单位
王子维 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
黎宇辉 湖北工业大学 机械工程学院武汉 430068 
童宇星 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
舒灏 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
刘奔 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
徐耀威 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
刘志昌 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
高颂 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
刘雄斌 湖北中烟工业有限责任公司武汉 430040
湖北新业烟草薄片开发有限公司武汉 430056
重组烟叶应用技术研究湖北省重点实验室武汉 430040 
摘要点击次数:
全文下载次数:
中文摘要:
      目的 开发一种新型烟草薄片成型试制设备,实现薄片自动成型、厚度可调、质量可控。方法 改变钢带和稠浆盒的运动方式;改良传统稠浆法烟草薄片成型工艺,包括剥离剂喷涂工艺、流浆成型工艺、热–风干燥工艺。通过对设备热–风干燥系统的工作过程进行流热耦合分析,并根据结果对热–风干燥系统的结构及参数进行优化,减少薄片在烘干过程中起皱、裂纹等缺陷的产生。结果 开发的稠浆法烟草薄片试制设备可制备0.15~0.3 mm厚度的烟草薄片,且薄片厚度均匀性好。优化热–风干燥系统前,烘干过程中烟草薄片主要区域的温度区间为37.7~59.6 ℃,优化后为50.1~64.2 ℃。结论 该设备减小了烟草薄片成型过程中薄片的尺寸波动,提高了薄片厚度均匀性。优化热–风干燥系统提高了烟草薄片温度分布均匀性,有利于烟草薄片成型质量的提高。
英文摘要:
      The work aims to develop a new type of trial production equipment for reconstituted tobacco sheet forming to realize automatic sheet forming, adjustable thickness and controllable quality. The movement mode of steel belt and raw material box was changed. The traditional thick paste tobacco sheet forming process was improved, including stripping agent spraying process, slurry forming process and heat air drying process. The fluid-thermal coupling analysis of the working process of the equipment heat air drying system was carried out, and the structure and parameters of the heat air drying system were optimized according to the results, so as to reduce the occurrence of wrinkles, cracks and other defects in the process of sheet drying. The trial production equipment for reconstituted tobacco sheet could produce tobacco sheet with a thickness of 0.15-0.3 mm, and the thickness uniformity of the sheet was good. Before optimization of the heat air drying system, the temperature range of the main area of tobacco sheet in the drying process was 37.7-59.6 ℃, and after optimization, it was 50.1-64.2 ℃. The equipment can reduce the size fluctuation of tobacco sheet in the forming process and improve the thickness uniformity of tobacco sheet. Optimizing the heat air drying system improves the temperature distribution uniformity of tobacco sheet, which is conducive to the improvement of tobacco sheet forming quality.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第21367549位访问者    渝ICP备15012534号-2

版权所有:《包装工程》编辑部 2014 All Rights Reserved

邮编:400039 电话:023-68795652 Email: designartj@126.com

    

渝公网安备 50010702501716号